Mechanical Properties Metric English Comments
Tensile Modulus 4.70 GPa

@Temperature 90.0 °C
682 ksi

@Temperature 194 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Tensile Modulus 4.70 GPa

@Temperature 23.0 °C
682 ksi

@Temperature 73.4 °F
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri..
Tensile Modulus 4.70 GPa

@Temperature 150 °C
682 ksi

@Temperature 302 °F
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 4.70 GPa

@Temperature 90.0 °C
682 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 4.70 GPa

@Temperature 120 °C
682 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 4.70 GPa

@Temperature 23.0 °C
682 ksi

@Temperature 73.4 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 4.70 GPa

@Temperature 150 °C
682 ksi

@Temperature 302 °F
LATI Later 4 K/30 PBT, 30% Carbon Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti..
Tensile Modulus 4.70 GPa

@Temperature 60.0 °C
682 ksi

@Temperature 140 °F
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 4.70 GPa

@Temperature 23.0 °C
682 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 4.70 GPa

@Temperature 100 °C
682 ksi

@Temperature 212 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66  (Unverified Data**)
Zytel® 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength, stiffness and im..
Tensile Modulus 4.70 GPa

@Temperature 90.0 °C
682 ksi

@Temperature 194 °F
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer
Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Tensile Modulus 4.70 GPa

@Temperature 90.0 °C
682 ksi

@Temperature 194 °F
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..
Tensile Modulus 4.70 GPa

@Temperature 60.0 °C
682 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..