Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.30 GPa @Temperature 60.0 °C |
624 ksi @Temperature 140 °F |
|
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Tensile Modulus | 4.30 GPa @Temperature 120 °C |
624 ksi @Temperature 248 °F |
|
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 4.30 GPa @Temperature 120 °C |
624 ksi @Temperature 248 °F |
|
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 4.30 GPa @Temperature 120 °C |
624 ksi @Temperature 248 °F |
|
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Modulus | 4.30 GPa @Temperature 120 °C |
624 ksi @Temperature 248 °F |
|
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Tensile Modulus | 4.30 GPa @Temperature 90.0 °C |
624 ksi @Temperature 194 °F |
|
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Metal stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE freeAvailability: A.. |
|||
Tensile Modulus | 4.30 GPa @Temperature 90.0 °C |
624 ksi @Temperature 194 °F |
|
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |