Mechanical Properties Metric English Comments
Tensile Modulus 4.20 GPa

@Temperature 120 °C
609 ksi

@Temperature 248 °F
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
Tensile Modulus 4.20 GPa

@Temperature 23.0 °C
609 ksi

@Temperature 73.4 °F
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 4.20 GPa

@Temperature 23.0 °C
609 ksi

@Temperature 73.4 °F
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Tensile Modulus 4.20 GPa

@Temperature 60.0 °C
609 ksi

@Temperature 140 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Modulus 4.20 GPa

@Temperature 120 °C
609 ksi

@Temperature 248 °F
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 4.20 GPa

@Temperature 150 °C
609 ksi

@Temperature 302 °F
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; ..
Tensile Modulus 4.20 GPa

@Temperature 60.0 °C
609 ksi

@Temperature 140 °F
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Tensile Modulus 4.20 GPa

@Temperature 23.0 °C
609 ksi

@Temperature 73.4 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 4.20 GPa

@Temperature 90.0 °C
609 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica..
Tensile Modulus 4.20 GPa

@Temperature 23.0 °C
609 ksi

@Temperature 73.4 °F
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 4.20 GPa

@Temperature 90.0 °C
609 ksi

@Temperature 194 °F
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 4.20 GPa

@Temperature 90.0 °C
609 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..