Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
ASTM-D638 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 60.0 °C |
334 ksi @Temperature 140 °F |
|
LATI Lasulf PSU Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 150 °C |
334 ksi @Temperature 302 °F |
|
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
|
LATI Lastilac AR-V0E ABS, Flame Retardant Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 60.0 °C |
334 ksi @Temperature 140 °F |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
|
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 120 °C |
334 ksi @Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Tensile Modulus | 2.30 GPa @Temperature 120 °C |
334 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |