Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.70 GPa

@Temperature 23.0 °C
537 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Tensile Modulus 3.70 GPa

@Temperature 23.0 °C
537 ksi

@Temperature 73.4 °F
LATI Larpeek 10 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.70 GPa

@Temperature 60.0 °C
537 ksi

@Temperature 140 °F
LATI Larpeek 10 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Tensile Modulus 3.70 GPa

@Temperature 150 °C
537 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 3.70 GPa

@Temperature 60.0 °C
537 ksi

@Temperature 140 °F
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Tensile Modulus 3.70 GPa

@Temperature 90.0 °C
537 ksi

@Temperature 194 °F
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 3.70 GPa

@Temperature 23.0 °C
537 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
Tensile Modulus 3.70 GPa

@Temperature 120 °C
537 ksi

@Temperature 248 °F
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Copyright © lookpolymers.com All Rights Reserved