Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.30 GPa @Temperature 150 °C |
479 ksi @Temperature 302 °F |
|
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Tensile Modulus | 3.30 GPa @Temperature 150 °C |
479 ksi @Temperature 302 °F |
|
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Improved thermal stabilization. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Tensile Modulus | 3.30 GPa @Temperature 120 °C |
479 ksi @Temperature 248 °F |
|
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Tensile Modulus | 3.30 GPa @Temperature 90.0 °C |
479 ksi @Temperature 194 °F |
|
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Modulus | 3.30 GPa @Temperature 90.0 °C |
479 ksi @Temperature 194 °F |
|
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North.. |
|||
Tensile Modulus | 3.30 GPa @Temperature 120 °C |
479 ksi @Temperature 248 °F |
|
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 3.30 GPa @Temperature -40.0 °C |
479 ksi @Temperature -40.0 °F |
1 mm/min; ISO 527-2 |
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE) Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r.. |
|||
Tensile Modulus | 3.30 GPa @Temperature -40.0 °C |
479 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8253 HS PA6 (Conditioned) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Tensile Modulus | 3.30 GPa @Temperature 120 °C |
479 ksi @Temperature 248 °F |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |