Polymer Property : Tensile Modulus = 290 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.00 GPa

@Temperature 120 °C
290 ksi

@Temperature 248 °F
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
LATI Latamid 6 E02 PA 6, Impact modified
Polyamide 6 (PA6). Toughened. Good impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A...
Tensile Modulus 2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 2.00 GPa

@Temperature 150 °C
290 ksi

@Temperature 302 °F
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 2.00 GPa

@Temperature 150 °C
290 ksi

@Temperature 302 °F
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Modulus 2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea..
Tensile Modulus 2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Modulus 2.00 GPa

@Temperature 60.0 °C
290 ksi

@Temperature 140 °F
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Tensile Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
ASTM D 638
Saint-Gobain Meldin® 2211 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Ser..
Tensile Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
Tensile Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
Tensile Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Tensile Modulus 2.00 GPa

@Temperature 150 °C
290 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..