Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 26.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 26.9 GPa

@Temperature 87.8 °C
3900 ksi

@Temperature 190 °F
0° Direction, Wet (2hr water boil immersion); ASTM D638 Type 1
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Tensile Modulus 26.9 GPa

@Temperature 93.3 °C
3900 ksi

@Temperature 200 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Modulus 26.9 GPa

@Temperature -53.9 °C
3900 ksi

@Temperature -65.0 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Tensile Modulus 26.9 GPa

@Temperature 71.0 °C
3900 ksi

@Temperature 160 °F
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric
Information provided by HexCel
Tensile Modulus 26.9 GPa

@Temperature 23.0 °C
3900 ksi

@Temperature 73.4 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement
Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel