Polymer Property : Tensile Modulus = 24.1 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 24.1 GPa

@Temperature -53.9 °C
3500 ksi

@Temperature -65.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Modulus 24.1 GPa

@Temperature 121 °C
3500 ksi

@Temperature 250 °F
0° Direction, Wet; ASTM D638 Type 1
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:..