Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 23.4 GPa @Temperature 21.1 °C |
3400 ksi @Temperature 70.0 °F |
0° Direction, Wet; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Modulus | 23.4 GPa @Temperature 82.2 °C |
3400 ksi @Temperature 180 °F |
0° Direction, Wet; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 23.4 GPa @Temperature 23.9 °C |
3400 ksi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure, 90min, 260°F; ASTM D638 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Tensile Modulus | 23.4 GPa @Temperature 23.9 °C |
3400 ksi @Temperature 75.0 °F |
0° Direction, Wet (2hr water boil); ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160.. |
|||
Tensile Modulus | 23.4 GPa @Temperature 23.9 °C |
3400 ksi @Temperature 75.0 °F |
Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Modulus | 23.4 GPa @Temperature 149 °C |
3400 ksi @Temperature 300 °F |
Wet; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Tensile Modulus | 23.4 GPa @Temperature 24.0 °C |
3390 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |