Mechanical Properties Metric English Comments
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer  (Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
Tensile Modulus 2.70 GPa

@Temperature 120 °C
392 ksi

@Temperature 248 °F
LATI Lapex A PES
Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Tensile Modulus 2.70 GPa

@Temperature 60.0 °C
392 ksi

@Temperature 140 °F
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 2.70 GPa

@Temperature 120 °C
392 ksi

@Temperature 248 °F
LATI Latamid 12 H2 G/30 PA 12, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 12 (PA12) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
LATI Latan 23UV POM
Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
LATI Latan 23UVE71 POM
Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Modulus 2.70 GPa

@Temperature 150 °C
392 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Modulus 2.70 GPa

@Temperature 150 °C
392 ksi

@Temperature 302 °F
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail..