Mechanical Properties Metric English Comments
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
LATI Lastilac 10 ABS/PC
ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 2.50 GPa

@Temperature 90.0 °C
363 ksi

@Temperature 194 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 2.50 GPa

@Temperature 120 °C
363 ksi

@Temperature 248 °F
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 2.50 GPa

@Temperature 150 °C
363 ksi

@Temperature 302 °F
LATI Laramid CE/60 PPA, 60% Mineral Reinforced
Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 2.50 GPa

@Temperature 150 °C
363 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe..
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 2.50 GPa

@Temperature 60.0 °C
363 ksi

@Temperature 140 °F
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;..
Tensile Modulus 2.50 GPa

@Temperature 120 °C
363 ksi

@Temperature 248 °F
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
LATI Latilon 30D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..