Mechanical Properties Metric English Comments
Tensile Modulus 2.20 GPa

@Temperature 60.0 °C
319 ksi

@Temperature 140 °F
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Tensile Modulus 2.20 GPa

@Temperature 60.0 °C
319 ksi

@Temperature 140 °F
LATI Lastilac 10 ABS/PC
ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Tensile Modulus 2.20 GPa

@Temperature 90.0 °C
319 ksi

@Temperature 194 °F
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Tensile Modulus 2.20 GPa

@Temperature 90.0 °C
319 ksi

@Temperature 194 °F
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Tensile Modulus 2.20 GPa

@Temperature 120 °C
319 ksi

@Temperature 248 °F
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Tensile Modulus 2.20 GPa

@Temperature 60.0 °C
319 ksi

@Temperature 140 °F
LATI Latamid 66 S/30 PA 66, 30% Glass Bead Reinforced
Polyamide 66 (PA66) based compound. Glass beads. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
LATI Latan 13 POM
Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Tensile Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..
Tensile Modulus 2.20 GPa

@Temperature 120 °C
319 ksi

@Temperature 248 °F
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Tensile Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app..
Tensile Modulus 2.20 GPa

@Temperature 23.0 °C
319 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad..
Tensile Modulus 2.20 GPa

@Temperature 60.0 °C
319 ksi

@Temperature 140 °F
LATI Latilon 30D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..