Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.1 GPa @Temperature 90.0 °C |
2630 ksi @Temperature 194 °F |
|
LATI Laticonther 80 GCE/650 PPS, Glass/Mineral Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Glass fibers / Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |