Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1670 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.5 GPa

@Thickness 0.0508 mm
1670 ksi

@Thickness 0.00200 in
RT; ASTM D638
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material
SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a ..
Tensile Modulus 11.5 GPa

@Temperature 60.0 °C
1670 ksi

@Temperature 140 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 11.5 GPa

@Temperature 120 °C
1670 ksi

@Temperature 248 °F
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 11.5 GPa

@Temperature 60.0 °C
1670 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; ..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 11.5 GPa

@Temperature 90.0 °C
1670 ksi

@Temperature 194 °F
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af..
Tensile Modulus 11.5 GPa

@Temperature 60.0 °C
1670 ksi

@Temperature 140 °F
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved