Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.3 GPa @Temperature 23.0 °C |
1640 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 11.3 GPa @Temperature 60.0 °C |
1640 ksi @Temperature 140 °F |
|
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 11.3 GPa @Temperature 60.0 °C |
1640 ksi @Temperature 140 °F |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 11.3 GPa @Temperature 120 °C |
1640 ksi @Temperature 248 °F |
|
LATI Latilub 66-15T K/30 PA66, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Tensile Modulus | 11.3 GPa @Temperature 23.0 °C |
1640 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Tensile Modulus | 11.3 GPa @Temperature 23.0 °C |
1640 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |