Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.2 GPa @Temperature 23.0 °C |
1480 ksi @Temperature 73.4 °F |
|
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Oil stabilized. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 10.2 GPa @Temperature 23.0 °C |
1480 ksi @Temperature 73.4 °F |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |