Mechanical Properties Metric English Comments
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
Tensile Modulus 10.0 GPa

@Temperature 90.0 °C
1450 ksi

@Temperature 194 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 10.0 GPa

@Temperature 60.0 °C
1450 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Low thermal expansion coefficient. Very high dimensional stab..
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi..
Tensile Modulus 10.0 GPa

@Temperature 90.0 °C
1450 ksi

@Temperature 194 °F
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced
Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation ..
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..
Tensile Modulus 10.0 GPa

@Temperature 60.0 °C
1450 ksi

@Temperature 140 °F
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 10.0 GPa

@Temperature 90.0 °C
1450 ksi

@Temperature 194 °F
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 10.0 GPa

@Temperature 23.0 °C
1450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
Tensile Modulus 10.0 GPa

@Temperature 90.0 °C
1450 ksi

@Temperature 194 °F
LATI Latamid 66 H2 K/20 PA 66, 20% Carbon Fiber Reinforced, Heat Stabilized