Polymer Property : Tensile Modulus = 1230 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66  (Unverified Data**)
Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po..
Tensile Modulus 8.50 GPa

@Temperature 120 °C
1230 ksi

@Temperature 248 °F
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 8.50 GPa

@Temperature 60.0 °C
1230 ksi

@Temperature 140 °F
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa..
Tensile Modulus 8.50 GPa

@Temperature 60.0 °C
1230 ksi

@Temperature 140 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 8.50 GPa

@Temperature 60.0 °C
1230 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Tensile Modulus 8.50 GPa

@Temperature 60.0 °C
1230 ksi

@Temperature 140 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 8.50 GPa

@Temperature 90.0 °C
1230 ksi

@Temperature 194 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 8.50 GPa

@Temperature 60.0 °C
1230 ksi

@Temperature 140 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610  (Unverified Data**)
Zytel® RS 30G30HSL BK038A is a lubricated, heat stabilized, 30% glass fiber reinforced black polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on po..