Mechanical Properties Metric English Comments
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6  (Unverified Data**)
Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Tensile Modulus 8.30 GPa

@Temperature 150 °C
1200 ksi

@Temperature 302 °F
LATI Latilub 66-15T K/30 PA66, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66
Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuP..
Tensile Modulus 8.30 GPa

@Temperature 23.0 °C
1200 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610  (Unverified Data**)
Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia..
Tensile Modulus 8.30 GPa

@Temperature 90.0 °C
1200 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..