Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.5 GPa @Thickness 0.0508 mm |
1670 ksi @Thickness 0.00200 in |
RT; ASTM D638 |
Rogers Corporation Syron™ 7100 Thermoplastic Circuit Material SYRON™ 7100 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7100 is thermally stable, with a .. |
|||
Tensile Modulus | 11.5 GPa @Temperature 60.0 °C |
1670 ksi @Temperature 140 °F |
|
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
|
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 120 °C |
1670 ksi @Temperature 248 °F |
|
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Tensile Modulus | 11.5 GPa @Temperature 60.0 °C |
1670 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
|
LATI Larton CE/60 PPS, 60% Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; .. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
|
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 90.0 °C |
1670 ksi @Temperature 194 °F |
|
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 60.0 °C |
1670 ksi @Temperature 140 °F |
|
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b.. |
|||
Tensile Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |