Mechanical Properties Metric English Comments
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Tensile Modulus 10.5 GPa

@Temperature 120 °C
1520 ksi

@Temperature 248 °F
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 10.5 GPa

@Temperature 120 °C
1520 ksi

@Temperature 248 °F
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &..
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 10.5 GPa

@Temperature 90.0 °C
1520 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 10.5 GPa

@Temperature 120 °C
1520 ksi

@Temperature 248 °F
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 10.5 GPa

@Temperature 120 °C
1520 ksi

@Temperature 248 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Modulus 10.5 GPa

@Temperature 60.0 °C
1520 ksi

@Temperature 140 °F
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri..
Tensile Modulus 10.5 GPa

@Temperature 90.0 °C
1520 ksi

@Temperature 194 °F
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 10.5 GPa

@Temperature 23.0 °C
1520 ksi

@Temperature 73.4 °F
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..