Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.50 kN/m | 8.56 pli | ASTM D-1876-72 |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |