Mechanical Properties Metric English Comments
Peel Strength 8.06 kN/m
46.0 pli
Tensile
Dielectric Polymers NT-490 Polyimide Label Stock  (discontinued **)
High temperature acrylic adhesive with thermal transfer imprintable polyimide film backing.Features: Meets ANSI standards for print contract signals and minimum reflectance ratios for bar code print..
Peel Strength 8.06 kN/m
46.0 pli
180°, Polyacrylic, Cotton duck failed during testing
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..