Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.380 kN/m | 7.875 pli | to Stainless Steel, 90°, 2 mil Al foil, 72 hr at 70°C; ASTM D3330 |
3M 9443NP Double Coated Tapes with Adhesive 700 Series 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat.. |
|||
Peel Strength | 1.380 kN/m | 7.875 pli | 90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330 |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.380 kN/m | 7.875 pli | Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 93015LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.380 kN/m | 7.875 pli | 90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |