Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.0408 kN/m | 5.9375 pli | Aluminum, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330 |
3M ScotchCal™ 3690E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | Aluminum, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330 |
3M ScotchCal™ 3698E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | 90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330 |
3M 7951 Hi-Performance Acrylic 300MP This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | 90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330 |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | PC, 180° peel, 2 mil Al foil backing, 72 hr dwell @ RT; ASTM D3330 |
3M 92015 Double Coated Tape with Adhesive 200MP 3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provide.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | PP, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330 |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9627 Adhesive Transfer Tape with Quick Bonding Adhesive 360 3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 880MSR Filament Tape Scotch® Filament Tape 880MSR is a high performance transparent filament tape reinforced along its length with continuous polyester-yarn filaments, which gives the tape a very high tensile strength... |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | 90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330 |
3M 9057MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.0408 kN/m | 5.9375 pli | to Steel |
3M Scotch® 393 General Purpose Cloth Tape Scotch® General Purpose Cloth Tape 393 is a polyethylene coated cloth backing coated with a rubber adhesive for moisture-proofing, duct sealing and general purpose applications.Information provided.. |