Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.982 kN/m | 5.60 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free .. |
|||
Peel Strength | >= 0.982 kN/m @Temperature 23.9 °C |
>= 5.60 pli @Temperature 75.0 °F |
Al/ |
Master Bond EP126 Two Component Toughened Epoxy Adhesive System Master Bond Polymer System EP126 is a two component toughened epoxy resin based high temperature resistant adhesive system with continuous service capability at 500°F and outstanding chemical resis.. |
|||
Peel Strength | 0.982 kN/m | 5.60 pli | High Impact Polystyrene, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.981 kN/m | 5.60 pli | to stainless steel, 180° peel test, rate of peel = 300mm/min at 25°C |
Kuraray SEPTON® A2 Hot Melt Adhesive Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block c.. |