Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.06 kN/m | 46.0 pli | Tensile |
Dielectric Polymers NT-490 Polyimide Label Stock
(discontinued **) High temperature acrylic adhesive with thermal transfer imprintable polyimide film backing.Features: Meets ANSI standards for print contract signals and minimum reflectance ratios for bar code print.. |
|||
Peel Strength | 8.06 kN/m | 46.0 pli | 180°, Polyacrylic, Cotton duck failed during testing |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |