Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 7.00 kN/m | 39.9 pli | Impact Peel |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |