Polymer Property : Peel Strength = 3.40 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 3.40 - 4.00 kN/m
19.4 - 22.8 pli
ISO 4578
Permabond TA435 Toughened Acrylic Adhesive & Initiator
PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli..
Peel Strength 3.40 - 4.00 kN/m
19.4 - 22.8 pli
ISO 4578
Permabond TA437 Toughened Acrylic Adhesive
PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-120H TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-620 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-626 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-626H TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-626L TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-626SH TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-626SL TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-690 TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 - 5.44 kN/m
19.4 - 31.0 pli
Initial (5 min.) PVC vs. PVC
Taiwan Sheen Soon Sheenthane® AS-690H TPU for PU Adhesive
Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations..
Peel Strength 3.40 kN/m
19.4 pli
Mylar Film; ASTM D-1876-72
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv..
Peel Strength 3.40 kN/m
19.4 pli
T-Peel (CRS St 1203, 0.5mm)
Dow BETAMATE™ 1045 Epoxy
BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent..
Peel Strength 3.40 kN/m
19.4 pli
Impact Peel
Dow BETAMATE™ 5103-2 Epoxy
BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste..