Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 28.0 kN/m | 160 pli | Impact Peel |
Dow BETAMATE™ 1496 V Epoxy BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle.. |