Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.80 - 3.60 kN/m | 16.0 - 20.5 pli | ISO 4578 |
Permabond ET510 Epoxy Resin PERMABOND ET510 is a two-part, 1:1 mixable epoxy adhesive. ET510 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas.. |
|||
Peel Strength | 1.80 - 3.60 kN/m | 10.3 - 20.5 pli | ISO 4578 |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Peel Strength | 1.80 - 3.60 kN/m | 10.3 - 20.5 pli | ISO 4578 |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |