Polymer Property : Peel Strength = 2.40 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.60 - 2.40 kN/m
9.13 - 13.7 pli
ASTM D903
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Peel Strength 1.60 - 2.40 kN/m
9.13 - 13.7 pli
ASTM D903
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Peel Strength 1.60 - 2.40 kN/m
9.13 - 13.7 pli
ASTM D903
Permabond 737 Cyanoacrylate, toughened
PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of..
Peel Strength 1.80 - 2.40 kN/m
10.3 - 13.7 pli
ISO 4578
Permabond ET514 Epoxy Resin
PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu..