Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.12 kN/m | 12.1 pli | Bond Strength (S1 to S2); Arlon SQA-TMS-011 |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Peel Strength | 2.12 kN/m | 12.1 pli | ABS, 180° |
3M Scotch-Weld™ 6111 Green Bulk only Adhesive Same as 6111 tan but green in colorInformation provided by 3M |
|||
Peel Strength | 2.12 kN/m | 12.1 pli | Open weave, polypropylene fabric, 180° |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |
|||
Peel Strength | 2.12 kN/m | 12.1 pli | ABS, 180° |
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M |