Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 12.6 kN/m @Temperature 21.1 °C |
72.0 pli @Temperature 70.0 °F |
|
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.06 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |
|||
Peel Strength | 12.6 kN/m | 72.0 pli | 180°, Aluminum |
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |