Polymer Property : Peel Strength = 11.31 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 1.983 kN/m
11.31 pli
to Stainless Steel, 90° peel, 5 mil aluminum foil backing, 72 hour 158°F (70°C)
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..