Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 10.9 kN/m | 62.0 pli | 180°, Glass |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 10.9 kN/m | 62.0 pli | 180°, ABS |
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |