Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.84 kN/m @Temperature 288 °C, Time 10.0 sec |
10.5 pli @Temperature 550 °F, Time 0.00278 hour |
Copper, After Solder Float; IPC-TM-650 2.4.8 |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | Bond Strength; ASTM D624 |
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | 90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330 |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour 158°F (70°C) |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | 90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.84 kN/m | 10.5 pli | Wood (Maple)-Unsupported Vinyl, 180°, Aging 1 Day @ RT |
3M Scotch-Weld™ 2262 Plastic Adhesive Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very .. |