Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.80 - 2.60 kN/m | 10.3 - 14.8 pli | ISO 4578 |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Peel Strength | 1.80 - 3.60 kN/m | 10.3 - 20.5 pli | ISO 4578 |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Peel Strength | 1.80 - 2.60 kN/m | 10.3 - 14.8 pli | ISO 4578 |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Peel Strength | 1.80 - 3.60 kN/m | 10.3 - 20.5 pli | ISO 4578 |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Peel Strength | 1.80 - 2.60 kN/m | 10.3 - 14.8 pli | ISO 4578 |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
Peel Strength | 1.80 kN/m | 10.3 pli | Aluminum Foil; ASTM D-1876-72 |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
Peel Strength | 1.80 - 2.40 kN/m | 10.3 - 13.7 pli | ISO 4578 |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |
|||
Peel Strength | 1.80 kN/m | 10.3 pli | Bell Peel |
Henkel Hysol EA 9394/C-2 Paste Adhesive System Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.Application: Structural Repair |