Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, 72 hr at 70°C; ASTM D3330 |
3M 3028EK Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Peel Strength | 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, 72 hr at 70°C; ASTM D3330 |
3M 9500B Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Peel Strength | 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, 72 hr at 70°C; ASTM D3330 |
3M 9500PC Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Peel Strength | 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, Acrylic Adhesive, 72 hr at 150°F; ASTM D3330 |
3M 9731 Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Peel Strength | 1.3257 kN/m | 7.5625 pli | Stainless Steel, 90°, Acrylic Adhesive, 72 hr at 150°F; ASTM D3330 |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |