Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.249 kN/m | 7.125 pli | Adhesion to Steel; ASTM D3330 |
3M 1450 Aluminum Foil Tape 3M™ Aluminum Foil Tape 1450 is an aluminum foil with transparent, high-tack, rubber adhesive.Information provided by 3M |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Adhesion to Steel; ASTM D3330 |
3M 1450 General Purpose Aluminum Foil Tape High tack adhesive for good, instant adhesion to many surfaces.Information provided by 3M |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9472 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9472 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9672 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9672 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9674 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9674 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 1.249 kN/m | 7.125 pli | to Steel; ASTM D3330 |
3M Scotch® 390 Polyethylene Coated Cloth Tape Scotch® Polyethylene Coated Cloth Tape 390 has a durable backing with a rubber adhesive used for applications requiring high strength and moisture resistance.Information provided by 3M |