Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.210 kN/m | 1.20 pli | Adhesion to steel; ASTM D1000 |
3M 2191FR EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Peel Strength | 0.210 kN/m | 1.20 pli | After 2 week exposure to 71°C, Vinyl-Gerfor NT to Treated plywood, 1 surface Bond |