Polymer Property : Peel Strength = 1.161 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7903FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7905 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7909 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..