Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.118 kN/m | 6.375 pli | ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9672LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Peel Strength | 1.118 kN/m | 6.375 pli | Stainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330 |
3M ScotchCal™ 3690E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Peel Strength | 1.118 kN/m | 6.375 pli | Stainless Steel, 180° Peel, Initial, 48 hr dwell at RT; ASTM D3330 |
3M ScotchCal™ 3698E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Peel Strength | 1.118 kN/m | 6.375 pli | Stainless Steel, Backside, 180° Peel, 2 mil Al |
3M XR4123 Double Coated Film Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Peel Strength | 1.118 kN/m | 6.375 pli | ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Peel Strength | 1.118 kN/m | 6.375 pli | ABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330 |
3M 9472LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |