Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | Backside, to Stainless Steel, 180° Peel, 2 mil Al |
3M XR8123 Double Coated Paper Tapes 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 1.01 kN/m | 5.75 pli | 72 hour RT glass, 90° peel, 5 mil aluminum foil backing |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |