Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.8925 kN/m @Treatment Temp. 204 °C, Time 3600 sec |
5.093 pli @Treatment Temp. 399 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.8925 kN/m @Treatment Temp. 204 °C, Time 3600 sec |
5.093 pli @Treatment Temp. 399 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.8925 kN/m @Treatment Temp. 204 °C, Time 3600 sec |
5.093 pli @Treatment Temp. 399 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.8925 kN/m @Treatment Temp. 204 °C, Time 3600 sec |
5.093 pli @Treatment Temp. 399 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.8925 kN/m @Treatment Temp. 204 °C, Time 3600 sec |
5.093 pli @Treatment Temp. 399 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |