Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 0.700 kN/m | >= 3.99 pli | ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket SOFT-SHIELD 5500 EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automatio.. |
|||
Peel Strength | 0.700 kN/m | 3.99 pli | 90° Acrylic Adhesive; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 3500 Plated-Fabric Wrapped Foam Economical EMI Shielding Gasket for Electronics Description: The SOFT-SHIELD® 3500 fabric cover foam [FOF] product family is a group of low-closure force EMI/EMC gaskets. SS3500 offers a low cost/ low closure force competitive solution for EMI s.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 177 °C, Time 3600 sec |
3.99 pli @Treatment Temp. 351 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 74.0 °C, Time 173000 sec |
3.99 pli @Treatment Temp. 165 °F, Time 48.0 hour |
95% RH, To Steel; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 177 °C, Time 3600 sec |
3.99 pli @Treatment Temp. 351 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 74.0 °C, Time 173000 sec |
3.99 pli @Treatment Temp. 165 °F, Time 48.0 hour |
95% RH, To Steel; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 177 °C, Time 3600 sec |
3.99 pli @Treatment Temp. 351 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 74.0 °C, Time 173000 sec |
3.99 pli @Treatment Temp. 165 °F, Time 48.0 hour |
95% RH, To Steel; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 177 °C, Time 3600 sec |
3.99 pli @Treatment Temp. 351 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 74.0 °C, Time 173000 sec |
3.99 pli @Treatment Temp. 165 °F, Time 48.0 hour |
95% RH, To Steel; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 177 °C, Time 3600 sec |
3.99 pli @Treatment Temp. 351 °F, Time 1.00 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.700 kN/m @Treatment Temp. 74.0 °C, Time 173000 sec |
3.99 pli @Treatment Temp. 165 °F, Time 48.0 hour |
95% RH, To Steel; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |