Polymer Property : Peel Strength = 0.578 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.578 kN/m
3.30 pli
[ppiw], Government Bond Strength; Arlon SQA-TMS-015
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape  (disco
2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical..
Peel Strength 0.578 kN/m
3.30 pli
[ppiw], Government Bond Strength; Arlon SQA-TMS-015
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape  (disco
1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v..
Peel Strength 0.578 kN/m
3.30 pli
Bond Strength; Arlon- SQA-TMS-015
Arlon 920-05B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular 0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Sel..
Peel Strength 0.578 kN/m
3.30 pli
Bond Strength; MIL-I-46852C
Arlon 920-10C##FR-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..
Peel Strength 0.578 kN/m
3.30 pli
Adhesion to Aluminum, anodized
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive
This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making ..
Peel Strength 0.578 kN/m
3.30 pli
Adhesion to ABS
3M Controltac™ IJ160C Graphic Film with Comply™ Adhesive
4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels ..
Peel Strength 0.578 kN/m
3.30 pli
Bond Strength; MIL-I-46852C
Arlon LW5015Y##-M1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.5 inch wide, 50 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll len..
Peel Strength 0.578 kN/m
3.30 pli
Polycarbonate, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Peel Strength 0.578 kN/m
3.30 pli
(S2 to S2), Bond Strength; Arlon SQA-TMS-011
Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo..
Peel Strength 0.578 kN/m
3.30 pli
Bond Strength; Arlon- SQA-TMS-015
Arlon 920-10B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..
Peel Strength 0.578 kN/m
3.30 pli
(S1 to S2) Bond Strength; Arlon SQA-TMS-011
Arlon 48360X005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111)..