Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.5425 kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.096 pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.5425 kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.096 pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.5425 kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.096 pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.5425 kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.096 pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Peel Strength | 0.5425 kN/m @Treatment Temp. 177 °C, Time 173000 sec |
3.096 pli @Treatment Temp. 351 °F, Time 48.0 hour |
To Aluminum; ASTM D1000 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |