Mechanical Properties Metric English Comments
Seal Strength <= 2700 g/25 mm
<= 2700 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating  (discontinued **)
Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Seal Strength 2700 g/25 mm
2700 g/in
seal bar 150°C.
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
Seal Strength 2700 g/25 mm
2700 g/in
seal bar 150°C.
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des..
Seal Strength <= 2700 g/25 mm
<= 2700 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging
Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene ..
Seal Strength 2700 g/25 mm
2700 g/in
seal bar 110°C.
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued